Dynamic test for low temperature reduction – disintegration – ISO 13930 (previously known as the Linder test)


Iron ore pellets are placed in a rotating tube and subjected to "tumbling during reduction". The samples are then subjected to a sieve analysis to determine the degree of disintegration.

  • Maximum temperature 600°C
  • Three heated zones over 715mm
  • Dual loop cascade control
  • Supplied with retort
  • Over-temperature protection
  • Flame failure gas safety system
  • Paperless data logging